To accelerate oxidation, spray the steel with a mixture of 1/3 hydrochloric acid and 2/3 water. Let it sit for 48 hours then rinse with clean water. You can repeat the operation if necessary.
Once the desired oxidation level is reached, we recommend applying an anti-rust product like Owatrol's Rustol to fix the oxidation.
Beware of rust drips during the oxidation phase, as they can damage the surface on which the steel elements are placed (tiling, wooden deck...)
Note:
Salt significantly damages your steel.
The superficial calamine plates are inherent to production and are an integral part of the product.